I know that when aluminum alloys are gas tungsten arc-welded (GTAW), usually we use alternating current (AC) because it give some sort of cleaning action. Can you explain what it is and how it works?

1 answer Reward0 Remaining Time 0 Day

 I know that when aluminum alloys are gas tungsten arc-welded (GTAW), usually we use alternating current (AC) because it give some sort of cleaning action. Can you explain what it is and how it works?

Other answers

  • 0861788249

    0861788249 2017-02-23 09:31:43

    Sure, let’s try. But before I start, let me admit that this explanation is a bit of a simplification. If I were to give a strictly correct explanation, it would take a lot more space than I have here. Also the following explanation will be of more practical use. So I’ll ask forgiveness in advance from all the physicists out there and proceed. It isn’t actually the AC that gives the cleaning action; it’s the part of the AC cycle when the tungsten electrode is positive. At these times the electrode is said to be the cathode in the circuit (the work is the anode), so this process sis called cathodic cleaning. When the tungsten is positive, electrons flow from the work to the tungsten. At this time, the arc uses most of its energy to heat the tungsten and produces shallow penetration. However, a counterflow of current—made of ionized atoms of shielding gas—also exists. For the moment let’s assume the shielding gas is argon. These ions, formed in the 10,000-degree-F-plus arc, have a positive charge and are attracted to the work surface, which at this time is charged negatively. So they accelerate because of the voltage difference and hit the work surface. The easiest way to understand this phenomenon (here comes the simplification) is to visualize the argon ions as sandblasting the surface of the aluminum and cleaning the oxide from it. So the electrode-positive part of the AC cycle gives us cathodic cleaning to remove the oxide from the surface of the aluminum, which we need, but it doesn’t help give us penetration, which is what we want. The penetration comes from the part of the AC cycle in which the electrode is negative. So we use AC to get both. Back when GTAW power supplies generated a simple sine wave, we were constrained to use 50 percent electrode negative and 50 percent electrode positive. However, we don’t need 50 percent electrode positive to get adequate arc cleaning. With the advent of square wave power supplies around 1975, we could adjust the balance of the wave to get a higher percentage of electrode negative and a lower percentage of electrode positive. It was found that a balance of about 65 to 70 percent electrode negative and 30 to 35 percent electrode positive gave sufficient arc cleaning. It also gave more weld penetration and less tungsten heating than a 50 percent positive arc. Some newer power supplies can provide adequate arc cleaning with as little as 10 to 15 percent electrode positive. From the standpoint of efficiency, set the balance control on your power supply as far toward “Penetration” or “Negative” as possible while still maintaining adequate arc cleaning. The sandblasting analogy can help explain a few other phenomena. We all know that argon gas shielding gives more arc cleaning than helium. Why? Consider the difference between sandblasting with sand versus features. The heavier medium gives the best results. The same is true with shielding gases. The heavier gas molecule gives more arc cleaning. What about gas metal arc welding (GMAW)? Because aluminum GMAW normally is performed with the electrode positive at all times, we get a lot of arc cleaning. Whenever you gas tungsten arc-weld aluminum using AC or gas metal arc-weld aluminum, you should be able to see the evidence of arc cleaning. It should look like a bright, frosty stripe about 1/16 to 1/8 inch wide along each side of the weld bead. If you can’t see these cleaning lines, you’ve done something wrong.

    [ More ] [ Close ]
    reply
    Answer0861788249:
    Answer
More

Wococarbide

Member login

shuriyouwu
Forgot password?

Join free

Reset Your Password

Email:

SMS code:

Send Code

New Password:

Submit