Product Name is Fe102 iron base alloy powder. Iron based self soluble alloy is made by adding a certain amount of boron and silicon into iron-carbon alloy. It is usually used in mechanical parts with wear resistance and weak acid corrosion resistance under normal temperature of 500 ℃. Although the comprehensive performance of iron-based self soluble alloy is not as good as that of nickel based and cobalt based alloy, its wide source of raw materials and low price are the major advantages of its popularization and application.


Production method: atomization method

Shape: irregular

Application process: plasma surfacing

Iron content: ≥ bal

Grade: Fe102

Melting point: 1200 ℃

Hardness: HRC62

 

Bulk density: 4.7 g / cm3

Hall Flow: 17 s / 50g

matters needing attention:

1. Please weld in strict accordance with the requirements of oxygen acetylene flame spray welding process.

2. The powder of - 150 / + 53 um is suitable for medium and small spray guns, and - 106 / + 45 um is suitable for large spray guns.

3. If the alloy powder has moisture absorption, it should be dried (120 ℃ for 1 hour) before use.

 

For more information about the Fe based powder, 3D printing powder, spraying coat powder, or WC based powder, you may search online wococarbide. Wococarbide Provide various products and technical questions and answers.