current position:Information and data>Commonly used spray materials are:
WC-12Co
Performance and Application
Excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coating Better oxidation resistance than WC-Co and WC-NI and corrosion performance, excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and denser, smoother coating, better than other WC-based metal powders Oxidation and corrosion resistance properties, better chemical resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coatings better than WC-Co Corrosion resistance, excellent low temperature wear resistance, excellent high temperature cavitation resistance, excellent friction wear and sliding wear resistance, dense coating, use temperature up to 870 ℃ for the preparation of heat resistance, oxidation resistance, corrosion resistance and adhesion resistance Wear, high temperature gas corrosion wear, high temperature erosion wear, low stress abrasive wear, hard surface wear and other coatings.
For high temperature oxidation environment, good red hardness. Mainly used for high temperature resistance intermetallic adhesion wear, wear particle wear, corrosion resistance, fretting wear resistance, high temperature erosion wear resistance.
Microhardness
>1200
WC-10Co-4Cr
Performance and Application
Excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coating Better oxidation resistance than WC-Co and WC-NI and corrosion performance, excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and denser, smoother coating, better than other WC-based metal powders Oxidation and corrosion resistance properties, better chemical resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coatings better than WC-Co Corrosion resistance, excellent low temperature wear resistance, excellent high temperature cavitation resistance, excellent friction wear and sliding wear resistance, dense coating, use temperature up to 870 ℃ for the preparation of heat resistance, oxidation resistance, corrosion resistance and adhesion resistance Wear, high temperature gas corrosion wear, high temperature erosion wear, low stress abrasive wear, hard surface wear and other coatings.
For high temperature oxidation environment, good red hardness. Mainly used for high temperature resistance intermetallic adhesion wear, wear particle wear, corrosion resistance, fretting wear resistance, high temperature erosion wear resistance.
Microhardness
>1200
WC-CrC-Ni
Excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coating Better oxidation resistance than WC-Co and WC-NI and corrosion performance, excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and denser, smoother coating, better than other WC-based metal powders Oxidation and corrosion resistance properties, better chemical resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coatings better than WC-Co Corrosion resistance, excellent low temperature wear resistance, excellent high temperature cavitation resistance, excellent friction wear and sliding wear resistance, dense coating, use temperature up to 870 ℃ for the preparation of heat resistance, oxidation resistance, corrosion resistance and adhesion resistance Wear, high temperature gas corrosion wear, high temperature erosion wear, low stress abrasive wear, hard surface wear and other coatings.
For high temperature oxidation environment, good red hardness. Mainly used for high temperature resistance intermetallic adhesion wear, wear particle wear, corrosion resistance, fretting wear resistance, high temperature erosion wear resistance.
Microhardness
>950
WC-10Ni
Performance and Application
Excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coating Better oxidation resistance than WC-Co and WC-NI and corrosion performance, excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and denser, smoother coating, better than other WC-based metal powders Oxidation and corrosion resistance properties, better chemical resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coatings better than WC-Co Corrosion resistance, excellent low temperature wear resistance, excellent high temperature cavitation resistance, excellent friction wear and sliding wear resistance, dense coating, use temperature up to 870 ℃ for the preparation of heat resistance, oxidation resistance, corrosion resistance and adhesion resistance Wear, high temperature gas corrosion wear, high temperature erosion wear, low stress abrasive wear, hard surface wear and other coatings.
For high temperature oxidation environment, good red hardness. Mainly used for high temperature resistance intermetallic adhesion wear, wear particle wear, corrosion resistance, fretting wear resistance, high temperature erosion wear resistance.
Microhardness
>1100
Cr3C2-25NiCr
Performance and Application
Excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coating Better oxidation resistance than WC-Co and WC-NI and corrosion performance, excellent low temperature wear resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and denser, smoother coating, better than other WC-based metal powders Oxidation and corrosion resistance properties, better chemical resistance, excellent carbide dispersion promotes better microstructure, better deposition efficiency and density, smoother coatings better than WC-Co Corrosion resistance, excellent low temperature wear resistance, excellent high temperature cavitation resistance, excellent friction wear and sliding wear resistance, dense coating, use temperature up to 870 ℃ for the preparation of heat resistance, oxidation resistance, corrosion resistance and adhesion resistance Wear, high temperature gas corrosion wear, high temperature erosion wear, low stress abrasive wear, hard surface wear and other coatings.
For high temperature oxidation environment, good red hardness. Mainly used for high temperature resistance intermetallic adhesion wear, wear particle wear, corrosion resistance, fretting wear resistance, high temperature erosion wear resistance.
Microhardness
>850
Ni60
Performance and Application
It is used to prepare coatings such as heat resistance, oxidation resistance, corrosion resistance and adhesive wear resistance, high temperature gas corrosion wear resistance, high temperature erosion wear, low stress abrasive wear and hard surface wear.
Microhardness
>700
Stellite alloy
For high temperature oxidation environment, good red hardness. Mainly used for high temperature resistance intermetallic adhesion wear, wear particle wear, corrosion resistance, fretting wear resistance, high temperature erosion wear resistance.