       Brand Name Chemical Composition Preparation Method Particle Size Range Typical Application Data Download WOCO361 Nickel Coated Titanium Carbide Powder HV TiC12Ni An economical alternative to chemically coated 45/15μm WC-12Co powder. Has the same hardness and wear resistance as WC-12Co. Not recommended for use in corrosive environments. Working temperature<300℃ -- WOCO362 Titanium carbide cobalt chromium powder HV TiC28Co8Cr agglomeration sintered 45/15μm economical substitute for WC-10Co-4Cr powder. Has the same hardness and wear resistance as WC-10Co-4Cr. Can be used in wet and corrosive environments. Working temperature<500℃ -- WOCO461 Nickel-coated boron carbide powder AP Ni75B4C, adjustable Coating 106/45μm High hardness, more wear-resistant than Al2O3, TiC, Cr2O3, used for abrasive wear workpieces (sludge pump plunger), working temperature <900℃